| HS Code | 310613 |
| Type | Die Attach Film |
| Application | Semiconductor Packaging |
| Thickness | 5-50 micrometers |
| Adhesion Strength | 20-60 N/cm2 |
| Thermal Conductivity | 0.3-2 W/m·K |
| Curing Method | Thermal or UV |
| Dielectric Strength | ≥3 MV/cm |
| Storage Temperature | 5-25°C |
| Moisture Absorption | <0.5% |
| Outgassing | Low |
| Substrate Compatibility | Silicon, GaAs, Sapphire |
| Peel Strength | 10-25 N/cm |
| Color | Transparent or light yellow |
| Main Resin | Epoxy or Polyimide |
| Halogen Free | Yes |
As an accredited DAF (Die Attach Film) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DAF (Die Attach Film) is packaged in vacuum-sealed rolls, 8-inch width, 100 meters per roll, with moisture-barrier protection. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL) for DAF (Die Attach Film): Securely packs and ships approximately 400 rolls, ensuring protection from moisture, dust, and damage. |
| Shipping | The shipping of Die Attach Film (DAF) is conducted in controlled, moisture-proof and electrostatic discharge (ESD) safe packaging to maintain material integrity. DAF is typically shipped refrigerated or at room temperature, depending on manufacturer’s recommendations, and expedited transport is often used to minimize exposure to humidity, heat, or contaminants. |
| Storage | DAF (Die Attach Film) should be stored in a clean, dry environment at a temperature of 5–25°C, away from direct sunlight and humidity. It must be kept in its original, sealed packaging to protect against dust and contamination. Avoid stacking heavy items on top, and always follow manufacturer-specific storage guidelines to maintain material quality and performance. |
| Shelf Life | Die Attach Film (DAF) typically has a shelf life of 6 to 12 months when stored at recommended temperature and humidity conditions. |
As a dedicated manufacturer of DAF (Die Attach Film), we provide engineered materials to support high-reliability semiconductor assembly across several advanced downstream sectors. This section details specific industrial applications where our DAF line contributes to product performance, compliance, and manufacturing efficiency for global partners.
DAF is the industry standard adhesive in advanced IC packaging, ensuring reliable chip-to-substrate connections under high-density integration for mobile and computing devices. Our materials must consistently pass rigorous electric, mechanical, and reliability benchmarks required by large-volume device manufacturers. During multilayer IC packaging, DAF serves as both a structural adhesive and stress buffer, facilitating thin-profile device construction and enhanced circuit integrity.
Industry compliance standards
Typical usage ratio
Downstream process integration
Final product types
In the power electronics sector, DAF is specified for attaching IGBT and MOSFET chips to ceramic or leadframe substrates, especially for automotive and renewable energy applications. Here, material selection focuses on high thermal conductivity and mechanical stability over temperature cycling, as even microvoids or voiding lead to critical failures under high current operation. Process controls and data monitoring ensure all material performance aligns with automotive and industrial application needs.
Industry compliance standards
Typical usage ratio
Downstream process integration
Final product types
Camera module manufacturers specify DAF for chip bonding in compact imaging assemblies, where strict control over outgassing, die warpage, and contamination is required to safeguard sensor performance. The film's properties directly influence sensor alignment accuracy and resistance to moisture penetration, which are crucial for devices used in automotive, security, and mobile camera modules. Material traceability and line-level QC are enforced to meet stringent global standards.
Industry compliance standards
Typical usage ratio
Downstream process integration
Final product types
DAF is widely adopted in solid-state lighting for affixing LED dies onto metal-core or ceramic PCBs to achieve both thermal management and consistent luminous output over the device’s service lifetime. Material properties—particularly outgassing and optical clarity—are closely monitored during assembly to prevent lumen depreciation and color shift. Automated die handling systems maximize throughput while minimizing material waste.
Industry compliance standards
Typical usage ratio
Downstream process integration
Final product types
MEMS manufacturers use DAF as a critical assembly material in producing micro-electro-mechanical systems for physical sensing in automotive, consumer, and industrial applications. Here, adhesive reliability impacts not only device integrity but also mechanical and acoustic signal fidelity. Materials undergo ongoing batch testing for ionic purity, modulus, and humidity resistance to reduce field failures in harsh operation environments.
Industry compliance standards
Typical usage ratio
Downstream process integration
Final product types
Competitive DAF (Die Attach Film) prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618018036652 or mail to sales6@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618018036652
Email: sales6@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
We build die attach films for customers who depend on performance, stability, and reliability in microelectronic packaging. Our production lines turn out the DAF3100 series—built for those who assemble IC packages under demanding conditions. Unlike simple adhesives or tapes, a DAF comes loaded with engineered structure and a balance of tack, flexibility, and thermal support. You might notice differences in how one film handles silicon chips while another grips compound semiconductors—the goal remains consistent bond-line thickness, stress relief on the die, and no bleed onto critical interfaces.
Film quality starts with resin blends. Our process for DAF3100 uses a proprietary epoxy-acrylate combination, fine-tuned for temperature and cure profile during lamination. A dedicated coating method lays the film onto a precision carrier, achieving a release force that maintains pocket alignment but comes away cleanly under standard die attach pick-and-place. Each roll undergoes thickness checks; our target is ±2μm variance, giving the operator predictable pick height and uniformity across wafers—no guesswork, no shimming.
Operators in assembly lines talk about the handling difference. Some claim our film wets the die without lifting edges or “tenting,” even at fast cycle times. With low ionic content and controlled alpha emissions, our DAF3100 avoids unwanted conductive paths and corrosion under tight wire-bond layouts. Once cured, the crosslinked network holds up through reliability tests—thermal cycling, high-temperature storage, pressure cooker exposure. Early field feedback saw the film survive several hundred cycles from -65°C to 150°C, and it fends off delamination, which reduces early device failure rates.
We see a lot of interest in the 20μm, 30μm, and 50μm thicknesses. What changes between models are mainly mechanical properties and compatibility with die size. The 20μm model, for example, sits well on thin wafers or small chips, keeping profiles low for wirebonding beneath tight clearances. Go up to the 50μm, and the film can absorb more mechanical mismatch, especially with larger dies common in power devices. The difference in modulus matters: a lower modulus film cushions fragile dice, while stiffer films resist creep and shifting inside high-power packages.
Our films ship as pre-cut sheets and rolls up to 8-inch wafer formats. Surface properties matter—release liners must not shed particles during lamination, as that can seed voids or weaken die placement. We source liners that pass Tensile testing and dust monitoring, and the factory’s 10,000-class cleanroom keeps films free from outgassing elements and stray fibers. Inventory teams keep all lots lot-traceable, so any report of process variation can get tracked right back to the resin batch, curing oven run, and even specific operator shift.
Customers often ask about the right temperature to laminate DAF to their wafer. We calibrate release temperature curves to ensure easy transfer at below 90°C, well clear of the fragile interconnects on modern dies. Application temperature for final die attach typically sits around 150–180°C, with precise ramp rates so flux volatilizes fully without bubble defects. Our technicians trade notes with customers’ process engineers about changes in solder paste interaction, leadframe prep, or die texturing. Often, small tweaks in film thickness or cure time can save yields upwards of five percentage points in pilot runs.
Unlike films produced via outsourced mixing and coating, our controls remain hands-on from polymerization to slitting. If film tension drifts in climate-controlled storage, teams catch it at outgoing inspection. Seal failures or misaligned carriers never reach the end-user, because packaging practices in-house depend on lessons learned from years of customer returns—scratches from overly aggressive slitter blades, contamination from rollers not regularly cleaned, static from mismatched carrier liners.
Roll lengths run 100–500 meters depending on customer preference and lamination line throughput. We have had customers request bespoke hard-coating to resist scratch damage during automated wafer grinding; others want microperforated liners for easier manual alignment in early prototyping. Meeting these requests raises costs, but it drives material innovation within our R&D group as well. Few industries match semiconductors in the pace of change, and the ones who listen most closely to the production floor see their products endure.
DAF differs from classic paste adhesives in both chemistry and results. Many lines that once dispensed liquid adhesives found frequent rework or failed die-attach. Pasty adhesives form inconsistent bond thickness, and trapped air leads to high void rates. We designed DAF3100 for uniformity by spreading the film to target thickness within ±2μm before lamination, not after. Each layer supports high-volume, repeatable workflow with fewer print defects. Liquid materials can require long snap-curing, stressing throughput and leading to temperature gradients that encourage delamination—problems a DAF prevents with single-curing and strong interfacial bonding.
Strictly speaking, solid films also eliminate bleed—liquid adhesives can spill onto wirebond pads or creep from under large dice during curing. Die attach film anchors to the die, not the whole substrate, so it blocks contaminating neighboring circuits and leaves free field for fine-pitch interconnects. As dies shrink, the reliability advantage stacks up.
While some teams use conductive die attach pastes for certain package types, most consumer and automotive electronics avoid the risk of silver migration or ionic leakage. Our film stays inert under field voltages and does not generate mobile ions. This comes directly from the chemistry—an engineered organic network rather than inorganic filler-loaded compounds. From automotive control to consumer device logic, end users see reduced leakage, improved thermal budget, and no spatter or powdering as observed with solids-loaded adhesives.
A die attach film's life begins before the wafer leaves the fab, but its journey continues through temperature extremes, vibration, and aggressive autoclave soak after packaging. Our reliability lab tackled temperature cycling from the outset—batch after batch cycled for up to 500 thermal swings with almost no measurable change in shear strength. Film bonded to standard copper leadframes, gold-plated carriers, and even ceramic substrates each showed over 90% die retention in unbiased high-temperature storage lasting up to 1000 hours.
Concerns over outgassing—vapors contaminating neighboring chips—also drove the push for DAF over paste or liquid options. Many of our formulations pass total outgassing rates below 0.1% by mass at 250°C. This low volatility means nearby microstructures and MEMS move free of residue, filter clogging, or golden whiskering that can short-circuit next-generation assemblies.
Moisture resistance has real-world impact. Our DAF3100 survived 85°C/85%RH for 1000 hours (industry standard for harsh test), showing virtually no surface delamination and retaining electrical insulation. Cross-linked polymer chains in the film shield against ionic ingress—a major reason automotive and industrial circuits using our adhesives show low field failure rates, even after months in aggressive climates and through hundreds of power cycles.
Die attach film might look simple in a catalog, but integrating it into real assembly lines takes hands-on knowhow. In our experience, success rests as much on up-front process tuning as the film quality itself. For a start, die attach pressure must strike a balance between firm adhesion and stopping chip damage. Our training team has spent months on lines in South China and Malaysia, tweaking pick-and-place force profiles for different die sizes. Technicians learn to watch for symptoms—misaligned edges, bubbling at corners—then tune both equipment and film chemistry to improve yield.
We see higher throughput in lines that switched from paste to DAF, mostly due to reduced cleaning and lower die-misalignment. Users find less downtime scrubbing print heads, fewer returned wafers due to out-of-plane tilting, and less waste from non-wettable areas. DAF’s standardized thickness even allows customers to reduce calibration overhead between reel changes, meaning operators spend less time chasing yield drops and more time ramping volume.
Failures rarely trace to the film itself; they arise from upstream steps—improper die sawing, debris on the substrate, or insufficient dehydration of wafers. We constantly remind customers and partners to pay attention to humidity in storage; our shipping containers include desiccant and humidity indicators so each reel stays as dry as possible until use. If customers need tailored lamination speeds or surface treatments, our lines can be adjusted mid-run, based on a single production issue. Every tweak we make is an improvement echoed across hundreds of lines worldwide.
We don’t wait for new chip sizes or formats to land before modifying our films. Feedback from IDM fabs and OSATs feeds directly back to our material scientists. When one customer asked for extended shelf-life at high humidity, our chemists reformulated without plasticizers that could migrate. For wafer-level chip scale packages, where edge coverage is tight and tolerances unforgiving, we reworked the thermal cure profiles to lock down adhesive migration by more than 30%. Joint development agreements speed up prototype iterations, and customers know our process window documentation reflects factory realities, not just lab data.
A few years ago, market pressure emerged for low-temperature cure films suitable for sensors in medical and optical modules. We quickly pivoted our line to test new catalyst systems, halving cure temperature without sacrificing final bond strength. That changed the decision pattern for many customers: they could mount fragile sensor dice onto glass without cracked seals or browned surfaces. Feedback from field assembly drove our change; failures, remediation costs, and time-to-market delays always outweigh the modest incremental price of material improvement.
Close partnerships with users bring more than incremental progress. We see device architects collaborating directly with our applications team long before a product ever hits mass production. Instead of guessing at future use cases, chemists and engineers from both sides hammer out process windows in joint trials. The result—the final film spec fits not only today’s lines but also the next process generation, where demands for thinner, lighter, faster chips only intensify.
Test data drive our design choices. Early generations of our DAF fell short in wire pull tests for gold-bonded dies, especially after 500+ hours at 150°C. This direct feedback led to increasing crosslink density and fine-tuning filler content. After those changes, both thermal cycling and unbiased HAST scores improved, product qualification times dropped, and line yields climbed past previous benchmarks. Instead of theoretical modeling, we depend on ongoing customer audits—line visits, traced lot histories, long-form reliability studies. Reporting remains brutally factual; each process change sees publication in our customer advisory newsletters so that end users never second-guess the source.
Cost discussions dominate many first-time DAF adopters’ meetings. Operators often calculate materials cost per die, yet overlook rework rates, scrap, and downstream testing budgets. Comparing only invoice costs falls short. Teams who switched from paste-based adhesive systems to die attach film found they could boost first-pass yield over 97%, and reduce field failures by over 50% driven by less delamination and lower moisture ingress. The real saving happens after package shipment, not at material purchase.
We track the environmental pressures facing microelectronic manufacturers. Much of our DAF product line omits lead, antimony, and halogenated aromatics, helping customers meet REACH, RoHS, and automotive compliance without secondary remediation. Volatile organic compound (VOC) profile sits below regulatory thresholds, so you won’t see solvent vapor triggers at the lamination line. Waste reduction matters, which is why we moved to thinner carrier liners, reducing process scrap by nearly 20% since 2020. Our films don’t emit residual halides, so corrosion risk in storage and use stays minimal. Package reliability—measured in real-world burn-in data—tells us that cleaner, less aggressive adhesives directly extend device service life.
Worker safety remains a constant concern. Factory staff don’t handle any uncured resin or powdered filler—the entire compound comes as a dry film, no skin sensitization risk and easier wipe-up if trimmed scrap finds the shop floor. Customers with well-ventilated lines rarely need additional extraction beyond standard cleanroom protocols, and no noxious odors linger after lamination. This lets operators focus on process quality and throughput, not health impacts or monitoring airborne residues.
Some suppliers buy in semifinished films, slit to size, and relabel. Our production runs from monomer synthesis forward; raw resin compound gets mixed, cast, coated, and slit all inside one controlled line. Integrated production brings tighter lot-to-lot control—vital for high-volume customers tracking every micrometer and millisecond lost in assembly. Our continuous feedback loop from factory to field highlights shrinkage, modulus shifts, or adhesion drift early, not once a product returns from end-customer lines. If issues arise, we know exactly which batch, oven, or recipe adjustment sits at play.
Besides resin chemistry, we distinguish ourselves through post-lamination support. Our engineering support group sits in-house, tracking factory start-ups on each customer continent—whether troubleshooting pick-and-place accuracy or remote-tuning lamination temperature for high-elevation fabs. Many competitors send out standard lamination profiles or data sheets; we staff technicians who can remote in, review assembly footage, or schedule line audits. Continuity of service does more for customers’ line yield than spec tweaks or incremental modifications.
Customers in automotive, power modules, MEMS, and RF markets report fewer early failures after switching to DAF3100. This repeatable experience isn’t advertising—it comes from paired field test and bench validation, logged in joint reliability sites from Singapore to Dresden. Product advantage lies in stubborn adhesion under thermal, mechanical, and field stress—measurable both in test labs and under pulsed operating cycles in real devices.
Electronic packaging trends force everyone forward—smaller dies, higher I/O, lower z-height restriction, tighter thermal budgets. Demand for lower-void, cleaner attach calls for continued evolution of DAF materials. We see calls for laser-release films, gradient modulus layers, and smart adhesives tied to in-situ cure monitoring. Each new ask leads us right back to the lab, testing, iterating, and pushing results to production.
Die attach films have moved beyond a “glue” role. Now, they serve as engineered stress relievers, environmental shields, and a key differentiator in whether a package meets lifetime reliability or suffers early field return. We keep recasting our formulas in step with device design, always chasing higher yield, longer service, and lower environmental impact. And we do it with eyes and ears open to every operator complaint, process tweak, and real-world audit—never content with standing still.